1. Increase the production capacity without changing the mold.
PP material has better processing performance, which can improve the storage time, injection time, and mold opening and closing time of the product. Based on Mr. Wang's mold, the current wall thickness is about 1.0mm. Using the "quick machine" series of servo injection molding machines, the cycle can be shortened. The time has been increased to about 10 seconds, and the quality of the product has been greatly optimized to meet its physical properties such as anti-fall and pressing.
2. Start developing new molds.
Using mold technology, it is recommended to develop single-point feeding into double-point feeding, and optimize the wall thickness and reinforcing ribs of the product, which can generally reduce the weight of the product by about 20g, and ensure that the physical properties of the product are not disturbed.